Selection Guide

Read three numbers first: ratio, acid value, Tg.

Nine out of ten selection decisions on a polyester resin come down to these three numbers. The other four — viscosity, curing schedule, matting route, weathering class — are adjustments made after these are fixed. This page is about how to read them, not about deciding for you.

A grade number names a family, not a performance level.

Dongtu grades are four digits (2868, 2709, 5055A). A -1 suffix marks an adjusted version within the same family; a letter suffix marks a parallel specification. The digits carry no literal meaning — every producer numbers differently, so comparing grade numbers across suppliers is meaningless. Compare parameters instead.

Ratio notation in this industry means only two things:
50/50, 60/40, 70/30 — indoor hybrid, the mass ratio of polyester to epoxy. More epoxy gives better adhesion and corrosion resistance but poorer weathering.
93:7, 95:5, 96:4, 97:3 — outdoor, the ratio of polyester to curing agent (TGIC or HAA). A smaller number means less curing agent, lower acid value and better flexibility; a larger number means higher crosslink density, hardness and chemical resistance.
02 · Seven parameters

Every number answers one question.

ParameterUnit / typical rangeWhat it isWhen highWhen lowHow to use it
Ratio50/50 · 60/40 · 70/30 or 93:7 · 95:5Mass ratio of polyester to epoxy, or to curing agentMore epoxy → adhesion, corrosion resistance, lower cost; poorer weatheringMore polyester → weathering, flexibility, higher gloss; higher costFix the system first. If the ratio is wrong, every number after it is wasted.
Acid valuemgKOH/gMilligrams of KOH consumed per gram of resinHigh → higher crosslink density, hardness, chemical resistance, faster cureLow → more flexible, better levelling, but needs more curing agent and reacts slowerIt sets the curing agent dose. Miss it by five points and the film is either brittle or undercured.
Tg°C (glass transition temperature)The temperature at which the resin softens out of the glassy stateHigh → better storage, no blocking in summer, poorer powder flowLow → better levelling and low-temperature film formation, blocking risk in summerFor summer storage in southern China, watch stacking and transport temperature once Tg is below 55 °C.
ViscositymPa·s (test temperature must be stated)Resistance to flow in the melt, commonly measured at 175 °C or 200 °CHigh → anti-sag, suits thick film and textureLow → high levelling, mirror finish, suits thin filmCheck the temperature before the number. A 175 °C value and a 200 °C value are not comparable.
Curing°C / min (part temperature, not oven temperature)Temperature and time needed for full crosslinkingHotter → more energy, more overbake yellowingCooler → suits heat-sensitive substrates, but the window narrowsThick and dark parts heat slowly and need more time. The data sheet point is one equivalent cure, not the only solution.
Matting routeDry blend / single resin / physical mattingWhether low gloss comes from a reaction-rate difference or from a matting agentDry blend → stable gloss, fine hand feel, needs a matched pairSingle resin → simpler to run, gloss drifts with formulationFor a stable 5–20° matte, prefer dry blend; for 25–40°, a single resin is simpler.
Weathering classIndoor / general outdoor / super-durableGraded by years of exposure and gloss/colour retentionSuper-durable → curtain wall, profiles, outdoor structuresGeneral outdoor → guard rails, enclosures, outdoor furnitureFor building products exported to Europe, customers often ask for Qualicoat-type approval — confirm before quoting.

Ranges shown are industry typical, not grade specific — refer to each Dongtu data sheet. Values are not comparable across different curing systems.

03 · Pick by application

Eight common scenarios, eight systems.

Start from where the part is used, whether it needs certification, and whether the substrate tolerates heat. Then go into the system page for specific grades.

04 · Curing window

180 °C / 15 min on a data sheet is a point, not the whole story.

Curing is the integral of temperature over time. Lower the temperature and you extend the time; raise it and you can shorten the time, but beyond a limit yellowing and embrittlement begin. The chart below is schematic: the usable window is a band, and the width of that band is what separates a good system from a poor one.

Overbake: yellowing · embrittlement · gloss loss Undercure: impact and bend fail · poor chemical resistance Recommended Time / min Temperature / °C 0816 2432 150170 190210
Schematic curing window, not grade-specific data. A wider window is easier to run; a narrower window demands better oven uniformity.
05 · Frequently asked

Eight questions, each about a specific failure.

Is a higher acid value always better?

No. A high acid value raises crosslink density, hardness and chemical resistance, but flexibility and impact resistance drop and cost rises. Parts that get bent or hit hard — window frames, shaped sections — usually need a lower acid value.

Is a higher Tg always safer?

A high Tg mainly solves blocking in storage, at the cost of melt flow and levelling. For summer storage in southern China we suggest Tg ≥ 55 °C; if the part needs mirror levelling, balance Tg against flow and make up the difference with additives.

Why does one resin quote two viscosities at 175 °C and 200 °C?

Viscosity is extremely temperature sensitive. 175 °C is closer to the extruder and the spray melt; 200 °C is closer to some in-house test habits. Comparing two resins requires converting to one temperature, otherwise the numbers mean nothing.

The boiling-water test fails — should I change resin first?

Check three things first: whether cure is complete (time and part temperature), whether pretreatment is clean, and whether the formulation contains hydrophilic components. Most boiling-water failures are undercure, not a resin that dislikes water.

Where does overbake yellowing come from?

Too hot or too long, and ester bonds and residual end groups keep reacting and oxidising. Dark colours hide it; whites and pastels show it first. For thick parts, lower the oven temperature and lengthen time rather than the reverse.

Why does dry-blend matte gloss drift?

Dry blending forms a micro-rough surface from the reaction-rate difference between two resins. Mix uniformity, extrusion temperature and the curing window all amplify into gloss. To stabilise it, fix the mixing and extrusion parameters first.

Is texture created only by the texturing agent?

Mostly, but texture also depends on melt viscosity, particle size distribution and film build. The same agent gives a different depth once the resin or the film build changes. To reproduce a texture, fix all three variables.

Do I need to clean the line when changing system?

Yes. Cross-contamination between hybrid and outdoor systems hits weathering and gloss directly, and light-to-dark or matte-to-gloss changes also need cleaning. The purging compound in our additives range exists for this step; simply follow the equipment manual.

When in doubt, take a sample.

Tell us the substrate, film build, bake schedule and acceptance criteria. We match a resin at trial-powder grade for the application, with TDS and a suggested formulation.