Home/Applications/MDF & heat-sensitive substrates

MDF & heat-sensitive substrates

Medium-density fibreboard, plastic parts, modular interior panels. The substrate will not take 180 °C, so curing has to drop to 140–160 °C without sacrificing levelling or adhesion.

Typical film build
60–90 μm
Curing
140–160 °C / 10–20 min
System
Polyester / blocked isocyanate
Key figures
Low-temperature levelling · pinhole free

The 4 grades usually used here

Ordered by typical fit, not by sales volume. Your own substrate and process window still need to be checked item by item against the data sheet.

GradeSystemRatioAcidmgKOH/gViscositymPa·sTg°CFeatureTDS
P001 Polyester / Isocyanate 80:20 35-45 4000-6000 ≥60 Excellent leveling and wear resistance, high hardness, solvent resistance, can be used as transparent powder. On request
P002 Polyester / Isocyanate 85:15 25-35 3000-6000 ≥56 Excellent leveling, good weather resistance, and mechanical properties. On request
P003 Polyester / Isocyanate 83:17 30-50 3000-6000 ≥56 Low hydroxyl value resin, dry mixed or co-extruded with P004 to achieve low gloss coating. On request
P004 Polyester / Isocyanate 40:60 280-320 6000-9000 ≥50 High hydroxyl value resin, dry mixed or co-extruded with P003 to achieve low gloss coating. On request

Low-temperature curing costs reaction speed and film density. MDF also needs a conductive primer or preheat first, otherwise surface resistance is too high and powder pickup is poor — a step that is often overlooked.

Start with a 2 kg trial

Send substrate, film build, curing temperature and time, and gloss target. We match a grade to your window before shipping — no generic sample.

Request a sample