| Grade | System | Ratio | AcidmgKOH/g | ViscositymPa·s | Tg°C | Feature | TDS |
|---|---|---|---|---|---|---|---|
| 2868 | Polyester / TGIC | 93:7 | 28-32 | 4000-5000 | ≥66 | Excellent flow | TDS |
| 2700 | Polyester / TGIC | 90:10 | 50-55 | 4000-5000 | ≥68 | Building-grade dry-blend matting resin | TDS |
| 2709 | Polyester / TGIC | 90:10 | 50-55 | 4000-5000 | ≥68 | Building-grade dry-blend matting resin | TDS |
| 2604 | Polyester / TGIC | 96:4 | 20-22 | 5000-6000 | ≥62 | Building-grade dry-blend matting resin | TDS |
| 2866 | Polyester / TGIC | 93:7 | 30-36 | 5500-7500 | ≥68 | Provides good surface appearance | TDS |
| 2600 | Polyester / TGIC | 96:4 | 20-22 | 5000-6000 | ≥62 | Building-grade dry-blend matting resin | TDS |